Multistage crack seal vein and hydrothermal Ni enrichment in serpentinized ultramafic rocks (Koniambo massif, New Caledonia)

Michel Cathelineau
Connectez-vous pour contacter l'auteur
Andrey Myagkiy
  • Fonction : Auteur
Benoît Quesnel
  • Fonction : Auteur
  • PersonId : 769401
  • IdRef : 193067455
Marie-Christine Boiron
Pierre Gautier
  • Fonction : Auteur
  • PersonId : 896698
Philippe Boulvais
  • Fonction : Auteur
  • PersonId : 840705
Marc Ulrich
Laurent Truche
  • Fonction : Auteur
Fabrice Golfier

Résumé

Sets of fractures and breccia sealed by Ni-rich silicates and quartz occur within saprock of the New Caledonian regolith developed over ultramafic rocks. The crystallization sequence in fractures is as follows: (1) serpentine stage: lizardite > polygonal serpentine > white lizardite; (2) Ni stage: Ni-Mg kerolite followed by red-brown microcrystalline quartz; and (3) supergene stages. The red-brown microcrystalline quartz corresponds to the very last stage of the Ni sequence and is inferred to have precipitated within the 50–95 °C temperature range. It constitutes also the main cement of breccia that has all the typical features of hydraulic fracturing. The whole sequence is therefore interpreted as the result of hydrothermal fluid circulation under medium to low temperature and fluctuating fluid pressure. Although frequently described as the result of a single downward redistribution of Ni and Mg leached in the upper part of the regolith under ambient temperature, the Ni silicate veins thus appear as the result of recurrent crack and seal process, corresponding to upward medium temperature fluid convection, hydraulic fracturing and subsequent fluid mixing, and mineral deposition.

Domaines

Géochimie
Fichier non déposé

Dates et versions

insu-01405480 , version 1 (30-11-2016)

Identifiants

Citer

Michel Cathelineau, Andrey Myagkiy, Benoît Quesnel, Marie-Christine Boiron, Pierre Gautier, et al.. Multistage crack seal vein and hydrothermal Ni enrichment in serpentinized ultramafic rocks (Koniambo massif, New Caledonia). Mineralium Deposita, 2017, 52 (7), pp.945-960. ⟨10.1007/s00126-016-0695-3⟩. ⟨insu-01405480⟩
186 Consultations
0 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More