Zinc partitioning between glass and silicate phases in historical and modern lead-zinc metallurgical slags from the PImageíbram district, Czech Republic Partage du zinc entre verre et phases silicatées dans des scories historiques et actuelles issues de la métallurgie du plomb dans le district de PImageíbram, République tchèque.
Résumé
Metallurgical slags of different ages resulting from Pb-metallurgy in the PImageíbram district (Czech Republic) have been studied. The chemical analysis (EPMA) of melilite, clinopyroxene, olivine and glassy matrix showed the following ZnO concentrations (in wt. %): 3.20-11.93 (melilite), 1.56 (clinopyroxene), 1.29-7.82 (olivine), 1.58-6.58 (glass). The Zn partition coefficient D = Cs / Cl between crystallized phases and coexisting glass was calculated. The values obtained are: 1.96-2.16 (melilite), 0.41 (clinopyroxene) and 0.79-1.19 (olivine). The distribution of zinc between the crystalline phases and glass depends on the phase assemblage, which reflects the blast furnace charge and temperature, as well as the cooling conditions of slags.
Domaines
Minéralogie
Origine : Fichiers éditeurs autorisés sur une archive ouverte
Loading...